Test "HDT"
The test determines the temperature at which a specified deflection occurs when a standard test specimen is subjected to a bending stress, to produce one of the nominal surface stresses in accordance with international standards.
This test is important for quality control and plastics research.
Test "VICAT"
The test determines the temperature at which a standard indenter penetrates 1 mm into the surface of a test specimen under load.
It is used to differentiate many types of thermoplastic materials with respect to their softening properties.
Standards: ISO 75, ISO 306, ASTM D 1525, ASTM D 648 and its equivalent.
We offer the following options: |
....................────────....................
.
.
Mechanical structure: Table type,
with lifting system automatic. Control mode: touch screen. Number of Measuring points.... .
. |
...............────────...............
.
HDT/V3216PC Control .
The tester is used to
determine the temperature deflection or the Vicat softening point. All samples are loaded ... .
. |
.............────────..............
.
Display mode:
LED. Control range temperature: temperature environment ~ 300ºC. Numbers test station ... .
|
..............────────...............
.
.
Control performed: Display
touch or PC. Accuracy: points temperature measurement multiple. Control range Of temperature... .
|
...................────────...................
.
HDT/V110.
The tester is used to
determine the temperature deflection or the softening point Vicat. All samples ... .
. |